Synthesis and characterization of Bi-doped zirconia for solid electrolyte

Kapil Sood, Kulvir Singh, O. P. Pandey

Research output: Contribution to journalArticlepeer-review

9 Scopus citations

Abstract

(100-x)ZrO2(x)Bi2O3 (x = 5, 10, 15) system has been synthesized by solid-state reaction technique. Tetragonal Bi7.38Zr0.62O12.31 phase has formed in all the samples after sintering at 850 °C for 24 h. Apart from this, ZrO2 and Bi2O3 are also identified as minority phases. The volume fraction of Bi7.38Zr0.62O12.31 phase increases with increasing concentration of Bi2O3. The AC conductivity plots exhibit phase transition at 570 °C and 460 °C for x = 10 and x = 15 samples, respectively. The maximum conductivity is observed (1.60 mS/cm) in x = 15 sample. These results are correlated and supported with microstructural and thermal analysis.

Original languageEnglish
Pages (from-to)549-554
Number of pages6
JournalIonics
Volume16
Issue number6
DOIs
StatePublished - Jul 2010
Externally publishedYes

Keywords

  • Ionic conductivity
  • Solid electrolytes
  • X-ray diffraction
  • Zirconia

Fingerprint

Dive into the research topics of 'Synthesis and characterization of Bi-doped zirconia for solid electrolyte'. Together they form a unique fingerprint.

Cite this